KAIST Nanostructures Copper Foil to Damp Dendrites in Anode-Free Cells
KAIST researchers structured copper current collectors with 300-nm tubes and a 10-nm MXene coating, quadrupling lithium-deposition area to fight dendrites in anode-free EV batteries.
Scope of change
- Results published 1 September in Advanced Functional Materials; KAIST professors Jinwoo Lee and Hee-Tae Jung led the work.
- Nanoscale tubular copper structures (300 nm diameter, 150 nm height) give roughly four times the lithium-deposition surface area of smooth foil.
- A ~10-nanometre MXene coating promotes a lithium fluoride-rich Solid Electrolyte Interphase to curb dendrite growth.
- A separate November 2025 KAIST team achieved 1,270 Wh/l in an anode-free lithium-metal battery, with 81.9% capacity retention after 100 cycles.
- No energy-density or cycle-life figures yet for the new approach; industrial scalability is unproven.

Four times the lithium-deposition surface area, from a copper foil restructured at the 300-nanometre scale — that is the core of a new anode-free battery approach from KAIST, published 1 September in Advanced Functional Materials.
Professors Jinwoo Lee and Hee-Tae Jung led the work, with Kyungpook National University and South Korea's National NanoFab Center contributing. The trade portal Electric Cars Report carried the findings.
What problem does this solve?
Anode-free cells deposit lithium directly onto a copper current collector during charging, instead of onto a graphite anode (the negative electrode in conventional lithium-ion batteries). Cutting the anode material trims cell weight and volume, which is why EV makers watch the technology closely.
The catch is uneven plating. Lithium builds up irregularly across the copper over repeated charge-discharge cycles, forming dendrites — branched structures that accelerate ageing and can trigger internal short circuits. The boundary layer between lithium and electrolyte, the Solid Electrolyte Interphase (SEI), can also destabilise.
How the copper was engineered
The team did not add excess lithium or thicker protective layers. Instead they attacked the copper surface itself.
- They applied Secondary Sputtering Lithography (SSL), a lithography process adapted from semiconductor manufacturing, to give the foil nanoscale tubular structures.
- Each tube measures roughly 300 nanometres in diameter and 150 nanometres in height, yielding about four times the deposition area of smooth copper.
- A roughly 10-nanometre coating of MXenes — a class of two-dimensional materials — sits on the structured surface.
The MXene coating, combined with the electrolyte used, promotes a lithium fluoride-rich SEI. Spectroscopic and electron-microscopic checks confirmed a uniform, nanoscale protective layer. The aim: fewer unwanted reactions between lithium and electrolyte, and suppressed dendrite growth.
Professor Jinwoo Lee's stated advantage: the method delivers uniform lithium deposition and a stable boundary layer without modifying the electrolyte composition or adding excess lithium.
What does this change for cell makers?
Not much yet, and the source is candid about it. Electric Cars Report gives no achieved energy density or cycle-stability figures for the new approach. Scalability of the lithography-based process to industrial production remains unproven.
The copper collector deserves attention regardless. A July study from Ruhr-Universität Bochum, the Helmholtz Institute Ulm and Karlsruhe Institute of Technology experimentally confirmed another ageing mechanism in lithium-metal batteries: lithium penetrates the copper collector and binds there permanently, cutting available capacity. Whether KAIST's nanostructuring counters that mechanism is unclear.
The technology ceiling is real. In November 2025, a separate South Korean team involving KAIST reached 1,270 Wh/l volumetric energy density with an anode-free lithium-metal battery — nearly double current EV lithium-ion cells, per chemie.de. That design used a polymer framework with embedded silver nanoparticles and a bespoke electrolyte. After 100 cycles it retained 81.9 per cent of original capacity, with 99.6 per cent average Coulombic efficiency (the share of charge recovered on discharge). The approach was validated in pouch cells.
What to watch next
Two open questions decide whether this leaves the lab: cycle-life and energy-density numbers for the SSL-structured copper, and a cost route for running semiconductor-style lithography over battery-scale foil. Watch for follow-up pouch-cell data from the KAIST group and any industrial partner announcement on collector manufacturing.
via electrive (Source)
More from Grace Kim
Show full bio
Staff writer covering people, launches and day-to-day practice in Automotive manufacturing and vehicle production at Autoplant Brief.
322 articles
Also circulated
- Fraunhofer LIMAC project targets lithium-metal cell durability
- Fraunhofer Tames Volume Swell in Aluminium Anode Cells
- Echion Taps Korea's ETS to Scale Niobium Anode Material XNO
- China Eyes Recycled EVs as Feedstock for Its EV Manufacturing Boom
- Maryland team links fast-charge slowdown to electrode drying